The drilling mud pump has poor working conditions and is a weak link in the drilling equipment. In actual production, drilling downtime due to mud pumping accident or damage can be encountered almost every day. Some people have made statistics in oil drilling: when the drill body is 2500M, 28.4% of the daily expenses are spent on the drilling mud pump, and 49.3% of the drilling is used to repair the drilling pump when there is no repairman. The vast majority of drilling mud pump accidents are caused by damage to wearing parts. According to statistics, the total footage of drilling in the Soviet Union in 1970 was 13.82 million meters, while 89,200 cylinder liners, 175,000 pistons and 238,000 valves were consumed. According to statistics of 73 drilling rigs in Shengli Oilfield in 1972, the total consumption of seven wearing parts of drilling pump was 1.57 million yuan, including 580,000 yuan for valves, 270,000 yuan for pistons, 300,000 yuan for cylinder liners, and 420,000 yuan for tie rods and packings. It can be seen that it is of great significance to study the damage mechanism of wearing parts and the influencing factors of their life, so as to improve the life and working reliability of wearing parts, and to reduce manpower and material consumption, improve drilling efficiency and reduce costs. This is also a key issue for the design of drilling rigs.  Practice shows that even the same wearing parts have different service life for different types of drilling pumps, that is, the same pump and the same wearing parts have different lifespans with and without improvement. This shows that after fully understanding the influence of various factors on the life of wearing parts, the life of wearing parts can be improved through improvements in structure, material and processing technology. The wearing parts of reciprocating mud pump mainly include cylinder liner, piston (or plunger and its packing), valve and valve seat, piston rod and its packing, etc. They are all reciprocating parts and the anti-grinding parts of their sealing friction pairs. They have two common characteristics: one is that the anti-grinding parts are elastic bodies, which can be deformed; the other is that they bear a certain pressure difference during the working process. Therefore, it is different from the friction pair formed by two rigid parts, and the study of its friction and wear laws is more difficult.

1 (1)

The flushing fluid delivered by the mud pump often contains a large number of abrasive particles, sometimes as high as 5-10%, and the particle diameter reaches 1.5-2.0mm, and its microscopic hardness reaches 180-230. When the wearing parts are reciprocating, due to the action of the pressure difference, the wedge-shaped liquid flow entrains the particles into the friction contact surface, so that the seals or rigid parts are scratched or grooved for a long time, and the wearing parts lose their normal working ability. Therefore, the normal wear of wearing parts generally forms a groove in the same direction as the reciprocating motion along the circumference of the friction pair parts, and in some places, traces of liquid erosion can be seen. The grooves on the elastic parts and rigid parts of the friction pair often correspond to convex and concave.

For the elastic parts in the friction pair, due to the unsatisfactory surface finish of the contact surface of the friction pair and the intrusion of abrasive particles, frictional resistance is generated in the reciprocating motion, and as the working pressure increases, the resistance also increases, and part of the energy is converted into heat energy. The temperature of the contact surface of the friction pair parts increases, and the heat transfer coefficient of the elastic rubber is very low. The heat is concentrated on the surface of the rubber parts, which causes the rubber to accelerate aging until it loses elasticity and no longer has sealing performance. Destruction of valve and valve seat: A large number of analysis results show that the life of the valve mainly depends on the working performance of the valve seal, so the damage and scrapping of the valve is mainly due to the premature failure of the rubber seal, so that there are tiny gaps on the working surface of the valve and the valve seat. The high-pressure liquid flow with abrasive particles pierces the working surface of the valve from small crevices and destroys it. The process can be roughly described as follows. When the mud pump is working, the dynamic load acts on the valve for many times, and the abrasive particles are firmly embedded in the working surface of the valve disc and the valve seat. Degree of dents. When the valve disc and the valve seat are in contact again, some abrasive particles will dent the formed dent, which will deepen and expand. As a result of so many repetitions, the surface of some metal layers is partially torn and elastically peeled off, and finally the valve and valve seat are damaged. According to the actual statistics, the scrapped valve disc due to the damage of the rubber sealing ring accounts for the total scrapped valve disc. 85% of the total number of valve discs damaged by this reason have grooves; the valve seats damaged by abrasive wear under the impact dynamic load account for 70% of the total number of valve seats scrapped. Circular wear marks appear on the surface.


Send Inquiry
Contact Us
  • Tel: +86-533-8171332
  • Fax: +86-533-8171332
  • Sales01@bp-mudpump.com
  • Add: Room 702, Block B, 105 Liuquan Road, Hi-tech Zone, Zibo, China